    Quote Originally Posted by Buckeye View Post
    So now we drop the kill coil and use store purchased coolants <shrug>
    NO because that opens a totally new can of worms, for the termite problem you have.
    I call it termite because something is eatting something.

    Best solution right now, is get rid of the eattable source.. ie... eK Nickle, and replace it with another vendor's nickle.. ie.. Swiftech, Koolance, DD, AquaCom, Bitspower.... someone who has a more and better refined plating process, and problem is solved.

    OR...

    Take your blocks to a local plater... have him do a batch job on all the blocks you wanted plated... go out on vacation with GF for the weekend... come back with done and completed blocks... and then your back in happy happy land.

    And this is what is pissing me off... because eK is saying no its not the nickle, everyone is thinking all vendors' nickle is bad.
    NO, EK HAS A BAD NICKLE SOLEY, NO OTHER VENDOR HAS THIS TYPE OF ISSUE.
    Last edited by NaeKuh; 06-06-2011 at 01:07 PM.
    Nadeshiko: i7 990 12GB DDR3 eVGA Classified *In Testing... Jealous? *
    Miyuki: W3580 6GB DDR3 P6T-Dlx
    Lind: Dual Gainestown 3.07
    Sammy: Dual Yonah Sossoman cheerleader. *Sammy-> Lind.*

    [12:37] skinnee: quit helping me procrastinate block reviews, you asshat. :p
    [12:38] Naekuh: i love watching u get the firing squad on XS
    Its my fault.. and no im not sorry about it either.

Bookmarks

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •