Quote Originally Posted by theseeker View Post


I took both blocks apart and the plating is completely gone in some spots with nothing but copper exposed. This is bizzare to me as I use demineralized H20! Maybe Eddie will chime in? I hope he does because I have two Nickel blocks for the 580's!
That's Feser? Oh...I do see "Eddie" spelled differently....is the Feser guy's name Eddie? I was thinking it was EK Eddy