There should not be a "inside of the braze" or "outside". When both base metals are at the correct temperature it should take ~1-2 seconds to touch the rod and it will flow. The trick is to get dis-simmiliar metals both to the correct brazing temp @ the same time.
Thanx, Walt. I understand. It's just going to take some practice for me to get this sorted out for myself.