There should not be a "inside of the braze" or "outside". When both base metals are at the correct temperature it should take ~1-2 seconds to touch the rod and it will flow. The trick is to get dis-simmiliar metals both to the correct brazing temp @ the same time.
None of the brazes on the HX look correct.


I forgot "you must" 
Reply With Quote
Bookmarks