That is galvanic corrosion at its finest. That happens with mixed metal loops, usually takes a while and yours looks really bad! Did you run straight distilled and biocide alone?

That picture is why I do not recommend running the Fusion HeatPipe that comes on the board. But, this like most of my posts in this thread will be ignored.
Did you mentioned this before?
Im kinda scare now, how many people out there are using the Striker II Fusion block? I know of many using the Maximus SE block and Blitz Extreme block, but I heard this time the S2E block has a different material (Got it from Triggers thread)

What exactly caused this? Can it really be the fusion block? I think Trigger mentioned he used this horribly liquid that looks like the main responsable.