I would use as thin a paste as you have ICD7 is kind of thick and takes time to spread cold and probably would skew the result.
One of the reasons to do it dry is that it reveals the imperfections. whetted with grease they fill in and in those void bondline areas the paste can be 2X or 3X thicker losing a good portion of performance. you will still have pretty much the overall psi that you had when it was dry but you lose the more important contact info.